The Scuffing Resistance of WC/C Coated Spiral Bevel Gears
PBN-AR
Instytucja
Instytut Technologii Eksploatacji
Informacje podstawowe
Główny język publikacji
angielski
Czasopismo
Key Engineering Materials
ISSN
1662-9795
EISSN
Wydawca
Trans Tech Publications Inc.
DOI
Rok publikacji
2014
Numer zeszytu
Strony od-do
36-40
Numer tomu
604
Link do pełnego tekstu
Liczba arkuszy
Słowa kluczowe
angielski
Bevel Gear, Coating, Scuffing
Streszczenia
Język
angielski
Treść
One of the main problems with the operation of spiral bevel gears is related to very severe conditions in the contact of the meshing teeth; therefore, lubrication is very difficult, which increases the risk of scuffing occurrence. One of the ways to achieve better scuffing resistance is by the deposition of a low-friction coating on the bevel gears teeth. Gear scuffing tests were performed using a bevel gear test rig designed and manufactured at ITeE-PIB. The authorial bevel gear scuffing test was performed. Specially designed, spiral bevel gears were used for testing. Two material combinations were tested: uncoated pinion - coated wheel and, for reference, both gears without coatings. The a-C:H:W (trade name WC/C) coating of DLC type was deposited on the wheel teeth. A mineral, automotive gear oil of API GL-5 performance level was used for lubrication. It is shown that the resistance to scuffing may be significantly improved when the a-C:H:W coating is deposited on the spiral bevel gear teeth.
Cechy publikacji
Oryginalny artykuł naukowy
Inne
System-identifier
PX-5698bad9810641ecf91a3205
CrossrefMetadata from Crossref logo
Cytowania
Liczba prac cytujących tę pracę
Brak danych
Referencje
Liczba prac cytowanych przez tę pracę
Brak danych